Differential Scanning Calorimetry (DSC) analysis is used to investigate thermal transitions in various polymer and some metal samples. NeXolve can perform measurement of specific heat capacity, temperature of phase changes, glass transition temperature and melt temperatures in the temperature range from -50 °C – 725 °C using a TA Instruments Q200 modulated differential scanning calorimeter.
Glass Transition Temperature (Tg); Melting Temperature (Tm); Crystallization Temperature (Tc). ASTM D7426-08; D3418-08; E1356-08, and other tests available.